Research and fabrication of high purity α-Al2O3 from Tan Rai aluminum hydroxide
DOI:
https://doi.org/10.51316/jca.2023.013Keywords:
Al(OH)3 Tan Rai, α-Al2O3, high purity α-Al2O3Abstract
This paper deals the effects of some factors on the fabrication process of high purity α-Al2O3 from Tan Rai Al(OH)3. The obtained results of surface morphology (SEM), crystal structure (XRD), composition (EDX) of the original Al(OH)3 and Al2O3 show that Al(OH)3 washed with CH3COOH 2N is best at 80oC, efficient Dissolution reached the highest when using 25% HCl, Al2O3 calcined at 1400oC for 2 hours. The obtained Al2O3 has the structure α-Al2O3, the high purity.
Downloads
References
P.-L. Chang, Y.-C. Wu, S.-J. Lai, F.-S. Yen, J. Eur. Ceram. Soc. 29 (2009) 3341–3348.
Y. Ueki, T. Kunugi, N.B. Morley, M.A. Abdou, Fusion Eng. Des. 85 (2010) 1824–1828.
P.G. Miney, P.E. Colavita, M.V. Schiza, R.J. Priore, F.G. Haibach, M.L. Myrick, Electrochem. Solid-St. 6 (2003) B42–B45.
N.D. Kerness, T.Z. Hossain, S.C. Mcguire, Appl. Radiat. Isotopes 48 (1997) 5–9.
Xuebing Hu et al Water Science & Technology: water supply (2018).
Wu Qin et al, Journal of Membrane Sciene 490 (2015) 160-168.
A. Amirsalari, S. Farjami Shayeteh Superlattices and microstructures 82 (2015) 507-524.
Chengchao Liu et al, RSC Advances 2 (2012) 8352-8358.
Jun Sung Lee, Hyun Soo Kim, No-Kuk Park, Tae Jin Lee, Misook Kang, Chemical Engineering Journal 230 (2013) 351-360.
Downloads
Published
Issue
Section
How to Cite
Share
Funding data
-
Trường Đại học Bách Khoa Hà Nội
Grant numbers T2020-SAHEP-031