Fined flint glass cullet (FFGC), hydrothermal reaction, Calcium Silicate Hydrate (CSH), Xonotlite, ecomaterialsAbstract
In this study, the effect of hydrothermal temperature of glass cullet (GC) and Ca(OH)2 was study. The batch-mixed sample with the Ca/Si 1.0 were hydrothermal reacted at different temperature such as 100, 150 and 180oC for 48 hour to find the suitable temperture to form the xonotlite. The data indicate that at 180oC for 48 hour, the peak of xonotlite at 2theta of 30 degree is highest, thus suggest for further study on the effect of hydrothermal reaction time to form the xonotlite.
Downloads
References
Pham TK, Kieu DTK, Do QM, Nguyen HT, Ly HA, Pham TTT. Journal of Science and Technology 4A 52 (2014) 198-204.
Pham T. K., Nguyen P., Nguyen T., Kieu K., Do M., Ly A. and Pham T., The 12th Vietnam-Japan international joint symposium, Can Tho City, Vietnam (2014) 73-78.
Do. M, Nguyen T, Pham K., The 11th international conference on ecomaterials (ICEM11) – Green Materials and Green Technology for Green “Monozukuri (Fabrication with heart), Hanoi, Vietnam (2013) 75-80
K. Pham.. RCME 29-30 Oct 2015, Bangkok, section 1C-3, pp. 1.
Lachowski, E.E., Murray, L.W. & Taylor, H.F.W.. Mineralogical Magazine 327 43 (1979) 333–336.
Merlino, S., Bonaccorsi, E., & Armbruster, T. Tobermorites;. American Mineralogist 10 84 (1999) 1613–1621.
O.A. Alawad, A. Alhozaimy, M.S. Jaafar, F.N.A. Aziz, A. Al-Negheimish. Int J Concr Structures Mater 3 9 (2015) 381-390.
F.P. Glasser, D.E. Macphee, E.E. Lachowski. MRS Proc 84 (2011) 331.
Black, K. Garbev, A. Stumm. Adv Appl Ceram 3 108 (2009) 137-144.
Y.-J. Zhu, X.-X. Guo, T.-K. Sham. Expet Opin Drug Deliv 2 14 (2017) 215-228
Downloads
Published
Issue
Section
How to Cite
Share
Funding data
-
Viet Nam National University Ho Chi Minh City
Grant numbers C2019-20-29